PIR insulation

Why does Therma TR27 have a different thermal conductivity from aluminium-faced boards?

At a glance

Therma TR27 is a PIR board with glass fibre facings on both sides, and its declared lambda depends on the thickness. The name of the core alone is therefore not enough to compare the thermal insulation of finished boards: the data for the selected variant must be read. The catalogue indicates flat roof and terrace build-ups with mechanical fastening, bonding or ballasting according to the system documentation. The glass fleece has a different function when joining layers than an aluminium facing. It is necessary to check how the surface of the board interacts with the first layer of the chosen waterproofing. A similar appearance of materials does not confirm that they are interchangeable, and the choice of adhesive and the preparation of the substrate still follow from the specific roof solution.

Beige facing over the yellowish core of a PIR board

First, identify the function

Overlooking the fact that a board with a fleece facing is not interchangeable with every PIR variant in any given bonded assembly leads to an error in the assessment. Well-chosen PIR boards allow the properties of the facing to be used without disregarding the requirements of a specific roof assembly. During the inspection, compare the type of substrate, the membrane variant and the documentation of the connection of all layers with the documentation or the condition before the change.

How to interpret the values

Comparing the thickness of TR27 requires two catalogue readings. The 100 mm board is assigned an RD of 3.70 m²K/W and a lambda value of 0.027 W/(m·K); for 120 mm the thermal resistance rises to 4.60 m²K/W and the lambda value is 0.026 W/(m·K). So it is not only the thickness that differs. These relationships must be preserved when comparing variants of polyurethane boards.

After changing the thickness of TR27, the lambda value and the declared thermal resistance must be read again, because the figure in the offer does not explain the conditions of use. A calculation with a single lambda value for both variants would distort the difference in their thermal resistance. Before assessing the savings promise, ask for RD 3.70 for 100 mm and RD 4.60 m²K/W for 120 mm in the variant comparison.

The glass fleece on TR27 is not an inferior version of the aluminium facing, but a different surface intended for interaction with specific layers of the roofing system. Its suitability is assessed within the adopted layer build-up, and the lambda value must come from the TR27 data, not from a general association with PIR. Separating the facing construction from heat conduction shows what really determines the choice of board.

A symptom does not always indicate the cause

The glass fibre facing of TR27 interacts with the layers of the adopted roofing system, which does not mean that the adhesive is arbitrary or that substrate preparation can be omitted. If there is a suspicion of a water or moisture problem, the surface on the TR27 facing intended for bonding the covering must be identified.

The surface to be bonded is prepared according to the requirements of the specific material set before the cause is attributed to the product name or facing. “Polyurethane foam” alone does not explain the problem, because approval for a specific bonded system does not cover any arbitrary compound with a similar name. The diagnosis should lead to a bond in accordance with the documentation of the correct set of board and waterproofing; before indicating the cause, compare the cleanliness and condition of the surface, the application requirements and the method of checking the finished bond with the history of the problem.

Where to look for discontinuities

The standard format of TR27 is 1200 × 600 mm, and the catalogue provides for square or rebated edges — the specific geometry and covering are confirmed for the order. In the case of a local discontinuity, inspect the joint between the boards in this format near the corner and the end of the roof flashing.

The edge of TR27 must be matched to the layout of the field and the support of the elements at the perimeter, even if the finished surface looks even and neatly finished. The type of joint must be checked, because cutting may obliterate the factory profile of the side that was to form the planned joint. The diagnosis of the cause is intended to allow the last rows to be set out before cutting the elements needed at the perimeter of the roof slope. To assess how the polyurethane insulation performs at this point, record the actual variant of the sides, the covering area and the way the new cut edges are closed.

Assessment of the material’s condition

TR27 declares at least 120 kPa at 10% deformation and reaction to fire class E. The loads and fire requirements of the entire roof assembly are assessed separately, and the product data sheet does not determine the local pressure at the service access to equipment above the boards.

A test result of 120 kPa at 10% deformation is not an approval for arbitrary use: the pressure in the service zone is assessed together with the protection and support of the TR27 layer. If anything is unclear, ask about the service traffic area, the support surface area and the classification conditions for the entire roof covering, rather than for a general assurance about the quality of the board.

Matching the solution to the problem

Compare the price of TR27 at an agreed thermal resistance and coverage scope, adding the fixing, auxiliary layers and the execution of details. When an offer refers generally to “polyurethane insulation”, check the TR27 pricing in the bonded system and in an alternative method of fixing the covering.

Compare the cost of the TR27 system at the same thermal resistance and with the roof completed to the same extent — otherwise a conclusion about cost-effectiveness or the completeness of an offer has no basis. A different fixing method changes material consumption and surface preparation, so without an itemised scope you do not know what you are actually comparing. A list of insulation packs does not show the actual cost of the system; you need the board thickness, the type of joint, the auxiliary layers and the flashings included in the contractor’s quote.

7 branches. Materials closer to your project.

Izoprofil.org map of seven branches offering sandwich panels, PIR boards and sheet metal
  • SEROCK — Dzierżenin 34 E
  • BŁONIE — ul. Sochaczewska 138A
  • RADOM — ul. Grobickiego 8
  • ŁÓDŹ — Natolin 8
  • OLSZTYN — Barczewo, ul. Prosta 9
  • WROCŁAW — ul. Jerzmanowska 10C
  • GORZÓW WLKP. — ul. Zielona 33/34

Check prices and availability: +48 500 409 109

Free quote

Materials for your project